1. Why should 25-13 series of welding wires and electrodes be used for the welding of austenitic stainless steel and carbon steel and low alloy steel (dissimilar steel welding)?

Answer: When welding austenitic stainless steel, carbon steel and low alloy steel in dissimilar steel welded joints, the weld metal must use 25-13 series of welding wires (309, 309L) and electrodes (Ao 312, Ao 307, etc.). If other stainless steel welding consumables are used, the martensitic structure will be formed on the fusion line of carbon steel and low alloy steel, which will cause cold cracks.

2. Why use 98%Ar+2%O2 shielding gas for solid stainless steel wire?

Answer: During MIG welding of solid stainless steel wire, if pure argon gas is used for protection, the surface tension of the molten pool will be large, and the welding seam will be poorly formed, showing a "hunchback" weld shape. Add 1-2% oxygen to reduce the surface tension of the molten pool, and the welding seam is smooth and beautiful.

3. Why is the surface of solid stainless steel wire MIG weld black?

Answer: MIG welding speed of solid stainless steel wire is fast (30-60cm/min), the shielding gas nozzle has run to the front molten pool area, the weld is still in a red-hot high temperature state, oxidized by the air, the surface is oxidized, and the weld is damaged. black. Pickling and passivation can remove black skin and restore the original surface color of stainless steel.


4. Why does the solid stainless steel wire need a pulsed power supply to achieve jet transition and spatter-free welding?

Answer: When MIG welding of solid stainless steel wire, φ1.2 welding wire, when the current I ≥ 260—280A, can realize the jet flow transfer; if the value is smaller than this value, the droplet is short-circuit transfer, and the spatter is large, so it is generally not used. Only when the MIG power supply with pulse is used and the pulse current is greater than 300A, the pulsed droplet transfer under the welding current of 80-260A can be realized without spatter welding.

5. Why is the flux-cored stainless steel wire protected by CO2 gas? Without a pulsed power supply?

Answer: At present, the commonly used flux-cored stainless steel welding wire (such as 308, 309, etc.), the flux formula in the welding wire is developed according to the chemical metallurgical reaction of welding under the protection of CO2 gas, so it cannot be used for MAG or MIG welding; Pulsed arc welding power source.
stainless steel

The above is the Selection Of Stainless Steel Wire we have listed for you. You can submit the following form to obtain more industry information we provide for you.

You can visit our website or contact us, and we will provide the latest consultation and solutions

Share to:

Send Inquiry

Home> Industry Information> Selection Of Stainless Steel Wire

Copyright © 2024 Shenzhen Lanejoy Technology Co.,LTD All rights reserved. Privacy Policy

We will contact you immediately

Fill in more information so that we can get in touch with you faster

Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.

Send